MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sipol Technipol® PA 2188 Thermoplastic Adhesive Co-polyamide
Categories: Polymer; Adhesive; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Description: Technipol PA 2188 is a co-polyamide based thermoplastic adhesive for automotive filter industry. In air engine filter manufacturing it can be used for edge sealing, for reinforcing beads and for pre-filter element bonding. Beside this, in oil engine filter manufacturing it can be used for first/last pleat bonding and for ecological end caps molding. It is characterized by a quick setting time, a good flexibility, a good wettability and a good chemical resistance. Technipol PA 2188 contains more than 80 % of raw materials coming from renewable resources (not-edible).

Information provided by SIPOL SpA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccASTM D 792
Viscosity 4.5 cP
@Temperature 230 °C
 8.0 cP
@Temperature 210 °C
 12 cP
@Temperature 200 °C
 18 cP
@Temperature 190 °C
Brookfield Viscosity 4.0 cP
@Temperature 232 °C
Cone/ plate Viscometer, Model Brookfield CAP 2000+.; MI 12
Storage Temperature 5.00 - 10.0 °C
 
Thermal PropertiesOriginal ValueComments
Softening Point 188 °CASTM D 3461
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 80.0 °CUnder Hopper
 170 - 195 °CCompression Zone
 195 - 210 °CMetering Zone
Feed Temperature 120 - 150 °C
Nozzle Temperature 210 - 220 °C
Die Temperature 210 - 220 °C
Shelf Life 12.0 Month
 
Descriptive Properties
ColorAmber
Suggested temperature profile for melters210-220°CPre-Heating Grills
 215-225°CTank
 230-240°CHose
 230-240°CNozzle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIPOL017 / 297142

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.