Product description: Grilon FG 40 NL natural 6025 is a modified, high viscosity polyamide 6. Compared to conventional polyamide 6 Grilon FG40 NL natural 6025 offers the following improvements:- Better gas barrier properties at elevated humidity and after pasteurization and sterilization
- Better optical and UV- barrier properties
- Better aroma barrier and flavor protection
- Better thermoforming and orientation properties
Application examples: Grilon FG 40 natural 6025 is suitable for production of mono and coextruded cast and blown films Grilon FG 40 natural 6025 is used for the manufacture of oriented films, sausage casings and deep-drawn films. It is also suitable for packaging such as meat cheese and fish (pouches, shells, covers) at elevated humidity levels.Information provided by EMS Grivory. |