MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NMG Atlas HPE100 Soteco Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset

Material Notes: Material has an IPN ("interpenetrating network polymer") structure. Due to this chemical structure the material can sustain high shear elongation before failure and allow a very low crack growth rate (high toughness). HPE is a thermoset material and shows higher temperature and styrene resistance than PVC and SAN. Thanks to its production process HPE is constituted by a very uniform and fine cell structure. The lower cell size leads to a lower resin intake in sandwich manufacturing.

Information provided by NMG Composites Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.100 g/ccASTM- D 1622
Water Absorption <= 1.0 %ISO 2896
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 25 %Shear elongation; ASTM-C273
Compressive Strength 1.30 MPaASTM- D 1621
Compressive Modulus 70.0 MPaASTM- D 1621
Shear Modulus 0.0170 GPaASTM-C273
Shear Strength 0.900 MPaASTM-C273
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0260 W/m-K
@Temperature 10.0 °C
ASTM- C 518
Maximum Service Temperature, Air 115 °C
Minimum Service Temperature, Air -180 °C
 
Descriptive Properties
Closed Cell Content>95%ISO 8301

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Jackon JACKOCELL® S232 Expanded Polystyrene Packaging and Shape Molding
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.005 Phosphoric Acid Anodized Aluminum Honeycomb
Evonik ROHACELL® 100 WIND-F Polymethacrylimide Foam
Eurofoam Porocell POR 300/100 Ethylene Octane Metallocene EPDM Foam
Elliott Company ELFOAM® P600 Polyisocyanurate Foam

PNMG920 / 230590

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.