MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mikro-Technik Mikrolen UHMW-PE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Ultra High Molecular Weight

Material Notes:

Properties:

  • very good impact resistance / high absorption at shock and impact stress
  • extremely high resistance against abrasive wear
  • good corrosion resistance
  • highly resistant at temperatures of -265°C up to +80°C (100°C) in relation to mechanical stress
  • Information provided by Mikro-Technik GmbH

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density >= 0.930 g/cc
    Molecular Weight 7.60e+6 g/mol
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore D 6015 sec
     613 sec
    Ball Indentation Hardness 36.0 MPa30 sec
    Tensile Strength, Yield >= 40.0 MPa
    Elongation at Break >= 350 %
    Izod Impact, Notched (ISO) >= 130 kJ/m²double notch
     NBsingle notch
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity >= 1.00e+14 ohm-cm
    Surface Resistance >= 1.00e+11 ohm
    Dielectric Strength 45.0 kV/mm
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 200 µm/m-°C
    @Temperature 23.0 - 80.0 °C
    Thermal Conductivity 0.410 W/m-K
    Melting Point 130 - 135 °CCrystalline melting range
     
    Descriptive Properties
    Tensile E-modulus6.8

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Zell-Metall Engineering Plastics Zellamid 1100
    Mitsubishi Chemical Advanced Materials TIVAR™ 88-2 UHMW-PE, Premium Lubricant Filled Lining Material
    Mitsubishi Chemical Advanced Materials TIVAR™ 88 UHMW-PE, Premium Glass Filled, Crosslinked Linings
    Overview of materials for Nylon 66/6
    Ensinger Tecast Vekton™ 6PA Black Unfilled Cast Nylon 6 (PA6)

    PMIKROT03 / 53102

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.