MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teijin Panlite® MN-3705 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: PC Grade. Availability: Africa, Middle East, Asia Pacific, Europe, Latin America, North America. Features: Bromine Free, Flame Retardant. Uses: Battery Cases, Electrical Parts. Forms: pellets. Processing Method: Injection Molding.

Information provided by Teijin Chemicals Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
Moisture Absorption 0.220 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 4.00 mm
Teijin method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 4.00 mm
Teijin method
Melt Flow 32.13 g/10 min
@Load 2.16 kg,
Temperature 280 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPaISO 527-2/50
Tensile Strength, Yield 60.0 MPaISO 527-2/50
Elongation at Break 100 %ISO 527-2/50
Elongation at Yield 7.0 %ISO 527-2/50
Tensile Modulus 2450 MPaISO 527-2/1
Flexural Strength 95.0 MPa2.0 mm/min; ISO 178
Flexural Modulus 2300 MPa2.0 mm/min; ISO 178
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 50.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+15 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°CISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 108 °Cunannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °Cunannealed; ISO 75-2/A
UL RTI, Electrical 80.0 °C
@Thickness 1.50 mm
UL 746
 80.0 °C
@Thickness 1.50 mm
UL 746
 80.0 °C
@Thickness 1.50 mm
UL 746
Flammability, UL94 V-2
@Thickness 0.400 mm
 V-0
@Thickness 0.800 mm
Glow Wire Ignition Temperature 825 °C
@Thickness 2.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength
Teijin Panlite® L-1225LM Polycarbonate
Teijin Panlite® LN-2250Z Polycarbonate
Teijin Panlite® ML-3500ZEH Polycarbonate
Teijin Panlite® MN-4800 Transparent Flame Retardant Polycarbonate

PTEIH944 / 191630

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.