System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Envalior Durethan® BKV 50 H3.0 000000 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 50% Glass Fiber Filled
Material Notes:
PA 6, 50% glass fibers, injection molding, heat-aging stabilized
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Bulk Density
0.700
g/cc
0.0253
lb/in³
ISO 60
Density
1.57
g/cc
0.0567
lb/in³
ISO 1183
Moisture Absorption at Equilibrium
1.5 %
1.5 %
50% RH; ISO 62
Water Absorption at Saturation
5.0 %
5.0 %
IOS 62
Linear Mold Shrinkage, Flow
0.0016
cm/cm
0.0016
in/in
150x105x3; 280 °C / MT 80 °C; 400 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0085
cm/cm
0.0085
in/in
150x105x3; 280 °C / MT 80 °C; 400 bar; ISO 294-4
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
225
MPa
32600
psi
5 mm/min; ISO 527-1,-2
Elongation at Break
3.0 %
3.0 %
5 mm/min; ISO 527-1,-2
Tensile Modulus
16.8
GPa
2440
ksi
1 mm/min; ISO 527-1,-2
Flexural Strength
360
MPa
52200
psi
2 mm/min; ISO 178-A
Flexural Modulus
15.5
GPa
2250
ksi
2 mm/min; ISO 178-A
Flexural Strain at Break
3.0 %
3.0 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
15.0
kJ/m²
@Temperature -30.0 °C
7.14
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
20.0
kJ/m²
@Temperature 23.0 °C
9.52
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)
95.0
kJ/m²
@Temperature 23.0 °C
45.2
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
95.0
kJ/m²
@Temperature -30.0 °C
45.2
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
Charpy Impact Unnotched
9.00
J/cm²
@Temperature -30.0 °C
42.8
ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
10.0
J/cm²
@Temperature 23.0 °C
47.6
ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched
1.50
J/cm²
@Temperature -30.0 °C
7.14
ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
2.00
J/cm²
@Temperature 23.0 °C
9.52
ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
20.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
11.1
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow
70.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
38.9
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point
222
°C
432
°F
10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi)
215
°C
419
°F
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
205
°C
401
°F
ISO 75-1,-2
Vicat Softening Point
>=
200
°C
@Load 5.10 kg
>=
392
°F
@Load 11.2 lb
120°C/h; ISO 306
>=
200
°C
@Load 5.10 kg
>=
392
°F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Glow Wire Flammability Index
650
°C
@Thickness 2.00 mm
1200
°F
@Thickness 0.0787 in
IEC 60695-2-12
Shrinkage, MD
0.020 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.020 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction 150x105x3; ISO 294-4
Shrinkage, TD
0.050 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.050 %
@Treatment Temp. 248 °F,
Time 4.00 hour
150x105x3; ISO 294-4
Processing Properties
Metric
English
Comments
Melt Temperature
280
°C
536
°F
injection molding
270
-
290
°C
518
-
554
°F
Mold Temperature
80.0
°C
176
°F
injection molding
80.0
-
120
°C
176
-
248
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
2.00
-
6.00
hour
2.00
-
6.00
hour
Moisture Content
0.030 - 0.12 %
0.030 - 0.12 %
Karl Fischer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Envalior Durethan® BKV 50 H3.0 000000 Nylon 6 (PA6), 50% Glass Fiber Reinforced, Conditioned
PLANW9428 / 208259
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.