MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Trigonox TMBH-L 1,1,3,3-Tetramethylbutyl hydroperoxide, 90% solution in solvent mixture
Categories: Other Engineering Material

Material Notes: Initiator (90% active ingredient in solvent mixture) for (co)polymerization of styrene and butadiene.

CAS number: 5809-08-5

EINECS/ELINCS No: 227-369-2

Applications: Trigonox TMBH-L may be used for the bulk and emulsion polymerization of vinyl monomers such as styrene, butadiene, acrylonitrile, acrylates and methacrylates. Trigonox TMBH-L can be activated by organic-soluble or water-soluble reducing agents and by metal compounds to accelerate polymerization and/or to reduce polymerization temperature.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Half-life  0.100
@Temperature 180 °C
0.100
@Temperature 356 °F
[hr]
 1.00
@Temperature 159 °C
1.00
@Temperature 318 °F
[hr]
 10.0
@Temperature 144 °C
10.0
@Temperature 291 °F
[hr]
Molecular Weight 146.2 g/mol146.2 g/mol
Storage Temperature -5.00 - 25.0 °C23.0 - 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 60.0 °C140 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay90.0-95.0 %
Color<20 Pt-Co
Content9.85-10.40 %Active oxygen
Content (%)10.94Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1220 / 286743

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.