MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials HOPG Graphite Monochromator  (discontinued **)
Categories: Carbon; Graphite

Material Notes: Advanced Ceramics' graphite monochromators are highly oriented forms of high purity pyrolytic graphite which diffract x-rays and neutrons with greater efficiency than any other material. In x-ray analysis, intensity is increased 3 to 5 times over that obtained with conventionally used crystals. A singly-bent focusing monochromator using graphite yields 3 times the intensity of lithium fluoride at equivalent resolution. GE Advanced Ceramics originally introduced, and still offers, graphite monochromators with the lowest mosaic spread (>= 0.4°) available.

Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.255 - 2.265 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000350 - 0.0000450 ohm-cmparallel (002) direction
 0.150 - 0.250 ohm-cmperpendicular (002) direction
 
Thermal PropertiesOriginal ValueComments
CTE, linear -0.100 µm/m-°C
@Temperature 20.0 °C
Slightly negative in parallel (002) direction.
CTE, linear, Transverse to Flow 20.0 µm/m-°C
@Temperature 23.0 °C
Thermal Conductivity 0.800 W/m-Kin perpendicular (002) direction
 16.0 - 20.0 W/m-Kin parallel (002) direction

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Graphite, Carbon, C
Momentive Performance Materials Pyrolytic Graphite (PG) Coating
Pyrolytic Graphite, Low Temperature Isotropic (LTI)
Momentive Performance Materials TC1050 Encapsulated Thermal Pyrolytic Graphite (TPG)
Momentive Performance Materials "PG" Pyrolytic Graphite

CADV36 / 426

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.