System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
A. Schulman BMC A50-EG Low Glass, Encapsulation Grade Molding Compound
Categories:
Polymer
;
Thermoset
;
Polyester, TS
;
Thermoset Polyester Glass Filled BMC
Material Notes:
BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.
Information provided by Bulk Molding Compounds, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.55
-
1.75
g/cc
Molded
Linear Mold Shrinkage
0.00070
-
0.0017
in/in
Mechanical Properties
Original Value
Comments
Hardness, Barcol
45 - 50
Tensile Strength
7100
-
9100
psi
Flexural Strength
13800
-
17800
psi
Flexural Modulus
680
-
880
ksi
Compressive Strength
16500
-
20500
psi
Izod Impact, Notched
5.00
-
7.00
ft-lb/in
Electrical Properties
Original Value
Comments
Dielectric Strength
391
-
441
V/mil
short time
Arc Resistance
>=
188
sec
Comparative Tracking Index
>=
500
V
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
>=
500
°F
Flammability, UL94
HB
Processing Properties
Original Value
Comments
Processing Temperature
280
-
330
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
A. Schulman BMC 1000 Thermoset Polyester, Food Grade
A. Schulman BMC 100 Thermoset Polyester, GP
A. Schulman BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
A. Schulman BMC 400 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
A. Schulman BMC 350 Thermoset Polyester, Medium Impact
PBMC920 / 123384
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.