MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane))  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Molded

Material Notes: BorPEX ME2510 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for crosslinkable pipes with superior flexibility.

BorPEX ME2510 is designed for the requirements in DIN 16 892/DIN 16 887 and prEN ISO 15 875 for hot and cold water pressure pipes, e.g. floor heating, radiator connections and for domestic hot and cold water supply.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.935 g/ccISO 1183
Melt Flow 1.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 15.0 MPaAt 50 mm/min; ISO/DIS 6259
Tensile Strength, Yield 2901 psiAt 50 mm/min; ISO/DIS 6259
Elongation at Break 180 %ISO/DIS 6259
Elongation at Yield 13 %ISO/DIS 6259
Modulus of Elasticity 0.630 GPaISO 527
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature -20.0 °C
ASTM D696
 140 µm/m-°C
@Temperature 20.0 °C
ASTM D696
 500 µm/m-°C
@Temperature 100 °C
ASTM D696
Specific Heat Capacity 2.10 J/g-°C
Thermal Conductivity 0.410 W/m-KDIN 52612
Vicat Softening Point 122 °CISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide))
Borealis HE2591 High Density Polyethylene Powder for Crosslinked Pipes (Pex-C (Irradiation))
Borealis HE2590 High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Borealis ME2592 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Westlake Plastics Lennite® Biocompatible Implant Grade UHMW-PE

PBOREA024 / 27331

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.