MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Toyobo CoolPoly® E3609 PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Product Description: CoolPoly E series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows design freedom in applications previously restricted to metals. The E series is electrically conductive and provides inherent EMI/RFI shielding characteristics.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Use: Automotive Applications; Lighting Applications

Automotive Specifications: GMG GMW17802P-PA6-T1

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccISO 1183
Water Absorption <= 0.10 %Equilibrium, 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0020 - 0.0060 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 95ISO 2039.2
Tensile Strength at Break 5220 psiISO 527-2/5
Elongation at Break 0.70 %ISO 527-2/5
Tensile Modulus 1.02e+6 psiISO 527-1
Flexural Strength 9280 psiISO 178
Flexural Modulus 1.20e+6 psiISO 178
Poissons Ratio 0.33ISO 527
Charpy Impact Unnotched 2.40 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.900 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 1.00 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.020 ohm-cmIEC 62631-3-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 12.0 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 29.0 µin/in-°FISO 11359-2
Thermal Conductivity 28.0 BTU-in/hr-ft²-°FThruplane; ASTM D1461
 120 BTU-in/hr-ft²-°FCrossflow; ASTM D1461
 170 BTU-in/hr-ft²-°FFlow; ASTM D1461
Melting Point 428 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 347 °FUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 410 - 464 °F
Middle Barrel Temperature 446 - 536 °F
Front Barrel Temperature 446 - 545 °F
Nozzle Temperature 419 - 536 °F
Zone 4 455 - 554 °FInjection
Melt Temperature 464 - 554 °F
Mold Temperature 212 - 284 °F
Drying Temperature 176 °F
Dry Time 2.00 - 4.00 hour
Back Pressure <= 50.8 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6271 / 310964

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.