Master Bond Polymer Adhesive Supreme 45HTQ is a two component, toughened, quartz filled epoxy compound for high performance structural bonding and casting. It is suitable for applications where long term exposure to temperatures from -60°F to +450°F is required. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |