MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Toyobo Celstran® TPU-GF40-01 AD3002 Black TPU, 40% Long Glass Reinforced
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced

Material Notes: Product Description: 40% long strand fiber glass reinforced thermoplastic polyurethane

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber

Form: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccISO 1183
Maximum Moisture Content 0.050
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 24800 psiISO 527-2/5
Elongation at Break 1.9 %ISO 527-2/5
Tensile Modulus 1.64e+6 psiISO 527-1
Flexural Strength 38600 psiISO 178
Flexural Modulus 1.51e+6 psiISO 178
Izod Impact, Notched (ISO) 16.0 ft-lb/in²
@Temperature -30.0 °C
ISO 180/1A
 19.0 ft-lb/in²
@Temperature 22.8 °C
ISO 180/1A
Charpy Impact, Notched 17.0 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 235 °FUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Processing Temperature 158 - 176 °FHopper
 482 - 500 °FHot Runner
Feed Temperature 68.0 - 122 °FInjection
Rear Barrel Temperature 464 - 482 °F
Middle Barrel Temperature 473 - 491 °F
Front Barrel Temperature 473 - 500 °F
Nozzle Temperature 473 - 500 °F
Zone 4 473 - 500 °FInjection
Melt Temperature 473 - 509 °F
Mold Temperature 158 - 194 °F
Drying Temperature 176 °F
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6263 / 310956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.