MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Weatherban™ PF5422 Ribbon Sealant
Categories: Polymer

Material Notes: 3M™ Weatherban™ Ribbon Sealants PF 5422 and PF 5423 are a supported synthetic rubber sealant in ribbon form. They offer a watertight, gasket-like seal in applications such as bedding glass, around window and door frames, etc. They can also act as a metal seam sealer in overlap seams, building panels, rain gutters, and can be used in conjunction with mechanical fasteners. They offer outstanding resistance to weathering, and develops good adhesion to glass, metal, and most other surfaces.

Features:

  • Protective liner and sealant are different widths for easy release.
  • Maintain tack at temperatures as low as 40°F (5°C) permitting application in unheated area.
  • Stays in position on vertical or overhead surfaces.
  • Easy hand layup – no special equipment needed.
  • Repositionable during application. Builds aggressive adhesion with time.
  • Solvent-free.
  • No shrinkage.
  • Vibration and sound dampening qualities.
  • Helps prevent bimetallic (galvanic cell action) corrosion, when placed between metal surfaces.
  • May be positioned side by side to achieve varying widths.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030
Tensile Strength at Break 0.228 MPa33.1 psi5"/Min
Elongation at Break 200 %200 %5"/Min
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33168 / 167915

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.