MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omni Plastics OmniTech™ ABS GR20 ABS, 20% Glass Reinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled

Material Notes: 20% Glass reinforced, general purpose; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Filler Content 20 %ASTM D2584
Melt Flow 4.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 69.0 MPaASTM D638
Elongation at Break 2.0 %ASTM D638
Flexural Strength 121 MPaASTM D790
Flexural Modulus 5516 MPaASTM D790
Izod Impact, Notched 80.0 J/m
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
@Thickness 3.17 mm
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Omni Internal Testing
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 400 - 480 °F
Middle Barrel Temperature 420 - 500 °F
Front Barrel Temperature 420 - 500 °F
Nozzle Temperature 420 - 500 °F
Melt Temperature 420 - 500 °F
Mold Temperature 80.0 - 140 °F
Drying Temperature 190 °F
Dry Time <= 4.00 hour
Moisture Content <= 0.020 %
Back Pressure 50.0 - 100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Omni Plastics OmniTech™ ABS GR10 ABS, 10% Glass Reinforced
Omni Plastics OmniTech™ ABS GR30 ABS, 30% Glass Reinforced
Omni Plastics OmniTuff™ CPP GRC20 Copolymer Polypropylene Glass Reinforced
Aclo Accutech ABS ABS831G20L Glass Reinforced
Hexcel® F161 Epoxy Resin, 120 Glass Fabric

POMNI5136 / 185282

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.