MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: Zytel® HTN54G35EF NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin, developed for electrical and electronics applications. It is also a PPA resin.

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccDAM; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 187 MPa
@Temperature 23.0 °C
DAM; ISO 527
Elongation at Break 2.7 %
@Temperature 23.0 °C
DAM; ISO 527
Tensile Modulus 10000 MPa
@Temperature 23.0 °C
DAM; ISO 527
Charpy Impact Unnotched 82.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Processing PropertiesOriginal ValueComments
Melt Temperature 325 °CDAM; Optimum
 320 - 330 °CDAM
Mold Temperature 85.0 - 135 °CDAM
Drying Temperature 100 °CDAM
Dry Time 6.00 - 8.00 hourDAM
Moisture Content <= 0.10 %DAM
 
Descriptive Properties
AppearanceNatural ColorDAM
FormsPelletsDAM
GenericPolyphthalamide (PPA)DAM
Material StatusPreliminary DataDAM
Part Marking Code>PA-IGF35<ISO 11469; DAM
 >PPA-IGF35<SAE J1344; DAM
Processing MethodInjection MoldingDAM
Product CategoryElectrical ResinsDAM
 Encapsulation ResinsDAM
 Glass Reinforced ResinsDAM
 Hydrolysis Resistant ResinsDAM
 Toughened ResinsDAM
Region Available - GlobalYesDAM
Resin IdentificationPA-IGF35ISO 1043; DAM

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN 55G55LWSF BK752A Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN 54G35HSLR BKB336 Polyphthalamide (PPA)

PZDSZ1436 / 140253

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.