MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Amietol® M12 Hygroscopic Liquid
Categories: Fluid

Material Notes: CAS No. 105-59- 9

Product Description: Amietol M12 (MDEA) is a clear hygroscopic liquid with an amine-like odor. The freshly distilled product is colorless, but prolonged storage may cause a yellowish discoloration.

Application/Uses:

  • Electronics industry
  • Paints, coatings & resins
  • Surfactants

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³
Viscosity Measure 99.05 cSt99.05 cSt
Molecular Weight 119.16 g/mol119.16 g/mol
Vapor Pressure 0.00000304 bar0.00228 torr
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 36.99 bar27750 torr
Critical Temperature 404 °C759 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 418.7 J/g180.1 BTU/lb
Specific Heat Capacity 1.72 J/g-°C0.411 BTU/lb-°F
Melting Point -21.3 °C-6.34 °FFreezing Point
Boiling Point 243.3 °C469.9 °F
Heat of Formation -91649 kJ/mol-91649 kJ/mol
Flash Point 138 °C280 °FClosed Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.46421.4642
 
Descriptive Properties
AppearanceColorless liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5067 / 222261

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.