MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Monprene® CP-32054G CLR Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-32054G CLR is a very soft clear low density thermoplastic elastomer gel designed for a variety of consumer product applications. Monprene CP-32054G CLR is a low density, high flow, high elasticity grade that is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Contact Clarity; High Elasticity; High Flow; Low Density; Low Hardness; Low Specific Gravity; Without Fillers

Uses: Consumer Applications; Footwear; Handles; Safety Equipment; Sporting Goods; Writing Instruments

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.880 g/cc0.0318 lb/in³ASTM D792
Melt Flow 27 g/10 min
@Load 2.16 kg,
Temperature 150 °C
27 g/10 min
@Load 4.76 lb,
Temperature 302 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8.0
@Time 1.00 sec
8.0
@Time 0.000278 hour
Injection Molded; ASTM D2240
Hardness, Shore OO 58
@Time 1.00 sec
58
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 2.76 MPa400 psiASTM D412
Tensile Stress at Strain 0.414 MPa
@Strain 300 %
60.0 psi
@Strain 300 %
ASTM D412
Elongation at Break 700 %700 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 171 - 193 °C340 - 380 °FMelt, Injection
Rear Barrel Temperature 127 - 160 °C260 - 320 °FInjection
Middle Barrel Temperature 149 - 171 °C300 - 340 °FInjection
Front Barrel Temperature 160 - 182 °C320 - 360 °FInjection
Nozzle Temperature 171 - 193 °C340 - 380 °FInjection
Zone 1 127 - 160 °C260 - 320 °FExtrusion
Zone 2 149 - 171 °C300 - 340 °FExtrusion
Zone 3 160 - 193 °C320 - 380 °FExtrusion
Zone 5 171 - 193 °C340 - 380 °FExtrusion
Die Temperature 171 - 193 °C340 - 380 °FExtrusion
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °FInjection
Injection Pressure 1.38 - 5.52 MPa200 - 800 psiInjection
Back Pressure 0.172 - 0.689 MPa25.0 - 100 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceClear/Transparent
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0829 / 237320

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.