- Fulacolor XW is a high performance reactive acid clay of exceptional whiteness designed to give excellent colour development.
- Fulacolor XW is compatible with all capsule technologies to produce a high definition instantaneous image. Low coarse particle content minimizes abrasion and capsule bleed, and extends filter-cycles.
- Fulacolor XW is a non-toxic material produced from natural material and consequently has extremely low environmental impact.
Information provided by Southern Clay Products |