System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LNP™ LUBRICOMP™ Compound ZL003 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories:
Polymer
;
Thermoplastic
;
Polystyrene (PS)
;
Polystyrene + Polyphenylene Ether, Unreinforced
Material Notes:
LNP LUBRICOMP ZL003 compound is based on Polyphenylene Ether / Polystyrene (PPE/PS) blend containing 15% PTFE. Added features of this grade include: Wear Resistant.
Features: Wear resistant
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.15
g/cc
0.0415
lb/in³
ISO 1183
Linear Mold Shrinkage, Flow
0.0089
cm/cm
0.0089
in/in
SABIC method
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
48.0
MPa
6960
psi
5 mm/min; ISO 527
Elongation at Break
8.3 %
8.3 %
5 mm/min; ISO 527
Tensile Modulus
2.25
GPa
326
ksi
1 mm/min; ISO 527
Flexural Strength
75.0
MPa
10900
psi
yield, 2 mm/min; ISO 178
Flexural Modulus
2.00
GPa
290
ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
5.00
kJ/m²
2.38
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
17.0
kJ/m²
8.09
ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
79.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
43.9
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow
81.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
45.0
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
130
°C
266
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi)
119
°C
246
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94
HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
UL 94
Processing Properties
Metric
English
Comments
Zone 2
290
-
300
°C
554
-
572
°F
Zone 3
300
-
310
°C
572
-
590
°F
Melt Temperature
300
-
305
°C
572
-
581
°F
Injection Molding
Mold Temperature
80.0
-
110
°C
176
-
230
°F
Drying Temperature
120
°C
248
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
29.0
-
43.5
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH81119 / 289066
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.