MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotch-Weld™ 1870 Industrial Adhesive
Categories: Polymer; Adhesive

Material Notes:

Features:

  • A fast drying, highly flexible adhesive with very long tack range and good water resistance
  • For bonding fabrics and most other lightweight materials with little or no tendency to stain or bleed through.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 26 - 30 %26 - 30 %
Brookfield Viscosity 450 - 1250 cP450 - 1250 cPRVF #3 sp @ 20 rpm @ 27°C
 
Mechanical PropertiesMetricEnglishComments
Peel Strength  0.526 kN/m
@Temperature 82.0 °C,
Time 1.81e+6 sec
3.00 pli
@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
 0.701 kN/m
@Temperature 66.0 °C,
Time 1.81e+6 sec
4.00 pli
@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
 1.23 kN/m
@Temperature 24.0 °C,
Time 259000 sec
7.00 pli
@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
 1.23 kN/m
@Temperature 24.0 °C,
Time 432000 sec
7.00 pli
@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
 1.23 kN/m
@Temperature 24.0 °C,
Time 605000 sec
7.00 pli
@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
 1.23 kN/m
@Temperature 24.0 °C,
Time 1.21e+6 sec
7.00 pli
@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
 1.23 kN/m
@Temperature 24.0 °C,
Time 1.81e+6 sec
7.00 pli
@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
 1.40 kN/m
@Temperature 24.0 °C,
Time 86400 sec
8.00 pli
@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
 2.63 kN/m
@Temperature -34.0 °C,
Time 1.81e+6 sec
15.0 pli
@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
 
Thermal PropertiesMetricEnglishComments
Flash Point -22.0 °C-7.60 °FTCC
 
Processing PropertiesMetricEnglishComments
Shelf Life 7.00 Month7.00 Month
 
Descriptive Properties
AppearanceTan
BaseSBR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34106 / 168853

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.