MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE EE-2280B Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink EE-2280B is a general purpose thermoplastic elastomer, available in BLK, designed for automotive exterior applications. Sarlink EE-2280B is a medium hardness, high density, UV stabilized grade with very good extrudability.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: UV Stabilizer

Features: Good Adhesion; Good Flexibility; Good Processability; Good Toughness; High Density; High Specific Gravity; Medium Hardness; Ozone Resistant; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 1183
Viscosity 310 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83ISO 868
 80
@Time 15.0 sec
ISO 868
Tensile Strength at Break 1170 psiFlow; ISO 37
 1830 psiAcross Flow; ISO 37
Tensile Stress at Strain 435 psi
@Strain 100 %
Across Flow; ISO 37
 551 psi
@Strain 100 %
Flow; ISO 37
Elongation at Break 610 %Flow; ISO 37
 720 %Across Flow; ISO 37
Tear Strength 220 pliAcross Flow; ISO 34-1
Compression Set 31 %
@Temperature 22.8 °C,
Time 79200 sec
ISO 815
 49 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 84 %
@Temperature 125 °C,
Time 252000 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Zone 1 380 - 400 °F
Zone 2 390 - 410 °F
Zone 3 400 - 420 °F
Zone 4 410 - 430 °F
Zone 5 410 - 430 °F
Die Temperature 420 - 440 °F
Screw Speed 30 - 100 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PSI 830 Polystyrene

PTEKNQ1037 / 237528

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.