MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Braskem UTEC7542F Ultra High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: UTEC7542F is an Ultra High Molecular Weight Polyethylene designed to achieve a unique particle size distribution. It is specifically intended for the battery separator markets, but is also useful for any application requiring either a low percentage of "large" particles or a higher percentage of
"fine" particles.
Applications: Lead acid battery separators, Synthetic Paper, Porous plastics.

Mechanical property data from double-notched specimens (14º v-notch on both sides) in accordance with ISO 11542-2.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.450 g/ccASTM D1895
Density 0.925 g/ccASTM D792
Particle Size <= 100 µmDp10; Laser Light Scattering
 125 µmAverage. Dp50; Laser Light Scattering
 <= 250 µmDp90; Laser Light Scattering
Viscosity Test 32 dl/gIntrinsic; ASTM D4020
Molecular Weight 9.50e+6 g/molaverage; Margolies
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 30.0 MPaASTM D638
Tensile Strength, Yield 17.0 MPaASTM D638
Elongation at Break >= 300 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmASTM D257
Surface Resistance >= 1.00e+12 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Melting Point 133 °CASTM D3418
 
Descriptive Properties
Particles (%)<1.0Laser Light Scattering. >300µm
 <4Laser Light Scattering. >250µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBRAS664 / 314057

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.