MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Telcar® TL-2363T Thermoplastic Elastomer
Categories: Polymer; Thermoplastic

Material Notes: Telcar TL-2363T is a UV resistant thermoplastic elastomer designed for outdoor applications requiring a soft, rubber-like feel. It is a high hardness grade that exhibits excellent abrasion resistance, suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Ablation Resistant; Brominated; Filled; Flame Retardant; Good Color Stability; Good Colorability; Good Flow; Good Gloss; Good Mold Release; Good Moldability; Good Processability; Good Processing Stability; High Flow; High Hardness; Light Stabilized; Lubricated; Medium Density; Slip

Uses: Consumer Applications; Flooring

RoHS Compliant:RoHS

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccASTM D792
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88
@Time 5.00 sec
Injection Molded; ASTM D2240
 90
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 1430 psiAcross Flow, Die C, 20 in/min; ASTM D412
 1810 psiFlow, Die C, 20 in/min; ASTM D412
Tensile Stress at Strain 878 psi
@Strain 100 %
Across Flow, Die C, 20 in/min; ASTM D412
 1060 psi
@Strain 300 %
Across Flow, Die C, 20 in/min; ASTM D412
 1180 psi
@Strain 100 %
Flow, Die C, 20 in/min; ASTM D412
 1380 psi
@Strain 300 %
Flow, Die C, 20 in/min; ASTM D412
Elongation at Break 520 %Across Flow, Die C, 20 in/min; ASTM D412
 550 %Flow, Die C, 20 in/min; ASTM D412
Tear Strength 267 pliAcross Flow, Die C, 20 in/min; ASTM D624
 329 pliFlow, Die C, 20 in/min; ASTM D624
Compression Set 44 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 85 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395B
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 20 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 370 - 410 °FInjection, Melt
Rear Barrel Temperature 340 - 380 °FInjection
Middle Barrel Temperature 350 - 390 °FInjection
Front Barrel Temperature 360 - 400 °FInjection
Nozzle Temperature 370 - 410 °FInjection
Zone 1 330 - 370 °FExtrusion
Zone 2 340 - 380 °FExtrusion
Zone 3 350 - 390 °FExtrusion
Zone 4 360 - 400 °FExtrusion
Zone 5 360 - 400 °FExtrusion
Die Temperature 374 - 410 °FExtrusion
Mold Temperature 77.0 - 150 °FInjection
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 50.0 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceBlue
 Colors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1645 / 238136

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.