MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Envision™ 3635-70 Diffuser Film
Categories: Polymer; Film

Material Notes: 2-mil, white vinyl film; Pressure sensitive adhesive adheres to rigid substrates; Create custom lighting effects for backlit applications; Control brightness and light distribution within light distribution within light boxes without hotspots; Available in three transmission levels: 30%, 50% and 60%; Use with florescent bulbs or LEDs. Typically for best results, 3M recommends using: films 3635-30 and 3635-70 for fluorescent lighting applications

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milwithout adhesive
 76.2 - 102 microns3.00 - 4.00 milwith adhesive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.2 MPa2490 psi
Peel Strength >= 0.526 kN/m>= 3.00 pliAdhesion to Acrylic panels
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 60 %60 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 16.0 °C>= 60.8 °FApplication Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Envision™ 3635-30 Diffuser Film

PMM34825 / 169572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.