MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AdvanSix Aegis® H73ZP Extrusion Grade Nylon 6  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as EU Directive 2002/72/EC. It possesses the combination of strength, toughness and thermo-forming properties associated with nylon 6 as well as excellent heat, chemical, and abrasion resistance.

Applications:

  • Processed Meat
  • Fresh Red Meat
  • Poultry
  • Fish
  • Cheese
  • Dried Food
  • Chilled Fruit Juices

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Permeability 992 g mil/ (m2 day)
@Temperature 38.0 °C
ASTM F1249
Specific Gravity 1.13 g/ccASTM D1505
Water Absorption 1.6 %in 24 hours
Moisture Absorption at Equilibrium 2.7 %at 50% RH
Water Absorption at Saturation 9.5 %
Oxygen Transmission Rate 40.3 cc/m²/day
Nitrogen Transmission 14.0 cc-mm/m²-24hr-atmcc/m²/day, No thickness given
Carbon Dioxide Transmission 72.8 cc-mm/m²-24hr-atmcc/m²/day, No thickness given
Viscosity Measurement 3.096% SAV
 73FAV; ASTM D789
Maximum Moisture Content 0.080
Melt Flow 4.5 g/10 min
@Load 1.00 kg,
Temperature 235 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 78.0 MPaMolded; ASTM D882
Film Tensile Strength at Yield, MD 40.0 MPaASTM D882
Film Tensile Strength at Yield, TD 30.0 MPaASTM D882
Film Elongation at Break, MD 339 %ASTM D882
 359 %ASTM D882
Elongation at Yield 4.2 %Molded; ASTM D882
Tensile Modulus 0.620 GPaTD; ASTM D882
 0.710 GPaMD; ASTM D882
 2.75 GPaMolded; ASTM D882
Flexural Strength 110 MPaMolded; ASTM D790
Flexural Modulus 2.67 GPaMolded; ASTM D790
Izod Impact, Notched 64.0 J/mMolded; ASTM D256
Tear Strength, Total 3290 NGraves, TD; ASTM D1004
 3530 NGraves, MD; ASTM D1004
Elmendorf Tear Strength MD 60200 gASTM D1922
Elmendorf Tear Strength TD 54000 gASTM D1922
Film Tensile Strength at Break, MD 90.0 MPaASTM D882
 90.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CASTM D3418
Maximum Service Temperature, Air 56.0 °CHeat Deflection Temperature; ASTM D648
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 230 - 260 °CCast Film
 246 - 254 °CTubular (Blown) Film
Adapter Temperature 260 °CTubular (Blown) Film
 260 - 266 °CCast Film
Die Temperature 490 °FTubular (Blown) Film
 500 °FCast Film
Melt Temperature 240 °C
 254 - 260 °CTubular (Blown) Film
 260 - 270 °CCast Film
Mold Temperature 80.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Puncture Index501 gm/milASTM D1306, MD
Puncture Strength1043 gASTM D1306, MD

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AdvanSix Aegis® H73QP Extrusion Grade Nylon 6
AdvanSix Aegis® H85QP Extrusion Grade Nylon 6
Overview of materials for Nylon 66, Film
AdvanSix Aegis® HCA73MP Nylon 6/6,6 Extrusion Grade Copolymer
AdvanSix Aegis® HCA73ZP Nylon 6/6,6 Extrusion Grade Copolymer

PALA09 / 23101

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.