MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 202 FR UV Nylon 6/6 (PA), Glass Fiber - Flame Retardant - UV Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: The RTP series of flame retardant, glass fiber reinforced nylon materials are designed to provide the optimal balance of strength, electrical and ignition resistance properties while exhibiting excellent processing characteristics. RTP 202 FR UV includes a UV stabilizer package to ensure good maintenance of these properties in outdoor applications.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.55 g/cc1.55 g/ccASTM D 792
Water Absorption 0.75 %
@Time 86400 sec
0.75 %
@Time 24.0 hour
ASTM D 570
Additive Loading 15 %15 %Primary Additive
Linear Mold Shrinkage 0.0025 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0025 - 0.0040 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D 785
Tensile Strength at Break 107 MPa15500 psiASTM D 638
Elongation at Break 2.0 - 4.0 %2.0 - 4.0 %ASTM D 638
Tensile Modulus 7.58 GPa1100 ksiASTM D 638
Flexural Strength 172 MPa25000 psiASTM D 790
Flexural Modulus 6.21 GPa900 ksiASTM D 790
Izod Impact, Notched 0.694 J/cm
@Thickness 3.20 mm
1.30 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.20 mm
10.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D 257
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 19.7 kV/mm500 kV/inShort Term; In Oil; ASTM D 149
Dissipation Factor 0.016
@Frequency 1e+6 Hz
0.016
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 243 °C470 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 221 °C430 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 277 - 299 °C530 - 570 °F
Mold Temperature 65.6 - 107 °C150 - 225 °F
Drying Temperature 79.4 °C
@Time 14400 sec
175 °F
@Time 4.00 hour
Moisture Content 0.20 %0.20 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 124 MPa10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PQZWA6342 / 92116

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.