MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Capella® HFC Auto
Categories: Fluid; Lubricant

Material Notes: Texaco Capella HFC Auto delivers value through:
  • Long service life and cleaner systems — Provides chemical and thermal stability.
  • High miscibility with R-134a — Allows ready lubricant flow in low temperature portions of the system.
  • Component wear protection — Provides excellent wear protection, particularly in bearing area
  • Suitable for retrofitting — compatible with minerals oils
  • Clean systems even under severe operation — Due to high solvency and thermal stability

Texaco Capella HFC Auto is a synthetic polyol ester based lubricant for automotive air conditioners.

Natural lubricity, combined with a special additive package, provides excellent wear protection.

It is miscible with refrigerant R-134a.

Texaco Capella HFC Auto is recommended for use:

  • in automotive air conditioners using hydrofluorocarbon (HFC) refrigerant, HFC-13a (R-134a)
  • in industrial applications with positive displacement or dynamic compressors that require a lubricant with a viscosity of 130 cSt at 40°C
  • with chlorinated refrigerants, including R-12, R-22 and R-502

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222062; MSDS Number: 9302

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.993 g/cc
@Temperature 15.6 °C
0.993 g/cc
@Temperature 60.0 °F
60/60°F
Viscosity Measurement 100100Viscosity Index
Saybolt Viscosity at 100°F 637 SUS637 SUS
Saybolt Viscosity at 210°F 72 SUS72 SUS
Kinematic Viscosity at 40°C (104°F) 122 cSt122 cSt
Kinematic Viscosity at 100°C (212°F) 13.1 cSt13.1 cSt
ASTM Color 0.500.50L; ASTM D1500
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.0200.020ASTM D974
 
Mechanical PropertiesMetricEnglishComments
Falex Load Test 136000 g300 lb14.2 mg of wear @ 5 h, R134a, Steel/Steel
 
Thermal PropertiesMetricEnglishComments
Pour Point -32.0 °C-25.6 °F
Flash Point 252 °C486 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 95 %
@Wavelength 400 nm
95 %
@Wavelength 400 nm
 
Descriptive Properties
AppearanceLight pale
Corrosion, Copper Strip1b1 h at 100°C
Miscibility of R-134a °F-2220% Lube lower

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Mobil Zerice 100 S Oil

WTEXA034 / 76913

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.