MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hardwire 3x2-4-12 Low Density Tape
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel; Metal Foam, Mesh, or Honeycomb

Material Notes: The 3x2 Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3x2 wire cord is made by twisting 5 individual wire together - three straight filaments wrapped by 2 filaments (All filaments are 0.01378 in diameter) at a high twist angle. The result is an easy to handle cord that combines great engineering values with excellent economics. If your application is tension dominated choose the 3x2.

Characteristics:

  • Best properties in tensile applications.
  • Excellent mix of engineering properties - Up to 8 KIPS/inch.
  • Great stiffness, instant wet-ability, and excellent conformability.
  • Works in all resins.
  • Asymmetric shape acts like a screw and gives mechanical bonding characteristics
  • Excellent fatigue properties in tension and in high-flex situations.
  • Great choice for extrusion and pultrusion applications.

All information provided by Hardwire, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0177 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 29400 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hardwire 3x2 Cord
ERG Aerospace Duocel® Aluminum Metal Foam
AISI 1005 Steel
Armacell Monarch® F-02001 Neoprene Based Rubber Foam
Cymat A35620SC 020SS Stabilized Aluminum Foam

NWIRE11 / 19997

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.