MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ TF 1641 PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • Meets ASTM D4894 Type IV, Grade 2 resin
  • Molding and ram extrusion powder very good free-flow properties
  • Good metering properties
  • Good mold filling behavior
  • Good electrical and mechanical properties
  • Very good surface quality of isostatic moldings
  • Excellent for small parts

Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.15 g/cc
@Temperature 23.0 °C
Sintering Molding; ASTM D4894-98a
Bulk Density 0.830 g/ccASTM D4894-98a
Particle Size 450 µmaverage; ASTM D4894-98a
Deformation 11 %2175 psi - permanent, 23°C, Sintering Molding; ASTM D621
 15 %2175 psi - 24 hrs, 23°C, Sintering Molding; ASTM D621
 17 %2175 psi - 100 hrs, 23°C, Sintering Molding; ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 27.58 MPaSintered Molding; ASTM D4894-98a
Elongation at Break 350 %Sintered Molding; ASTM D4894-98a
Tensile Modulus 87000 psiSintered Molding; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 98.4 kV/mmASTM D149-95a
 
Thermal PropertiesOriginal ValueComments
Melting Point 317 - 337 °Csecond; ASTM D4894-98a
 332 - 352 °Cinitial; ASTM D4894-98a
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -200 °C
Flammability, UL94 V-0
Shrinkage 2.8 %
@Temperature 23.0 °C
Sintering Moldings; ASTM D4894-98a

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ TF 1645 PTFE
3M Dyneon™ TF 1620 PTFE
3M Dyneon™ TF 1750 PTFE
3M Dyneon™ TFM™ 1700 PTFE
3M Dyneon™ TFM™ 1705 PTFE

PDYNE031 / 34839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.