MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Melinex® SWC Polyester Film, 48 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.480 mil
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 15000 psiASTM D882A
Film Tensile Strength at Yield, TD 15000 psiASTM D882A
Film Elongation at Break, MD 150 %ASTM D882A
Film Elongation at Break, TD 120 %ASTM D882A
Coefficient of Friction, Dynamic 0.40A-B; ASTM D1894
Film Tensile Strength at Break, MD 28000 psiASTM D882A
Film Tensile Strength at Break, TD 32000 psiASTM D882A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cm
@Temperature 25.0 °C
100 V DC 50% RH 1000 sec electrification time; ASTM D257
Surface Resistivity per Square 1.00e+15 ohm
@Temperature 25.0 °C
500 V DC @ 50% RH; ASTM D257
Dielectric Strength 10417 V/mil1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dielectric Breakdown 5000 V1/4" electrode 500 V/sec 25°C in air; ASTM D149
Dissipation Factor 0.0044
@Frequency 100 Hz,
Temperature 25.0 °C
ASTM D150
 0.0066
@Frequency 1000 Hz,
Temperature 25.0 °C
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 3.0 %
@Temperature 190 °C,
Time 300 sec
Unrestrained
Shrinkage, TD 1.0 %
@Temperature 190 °C,
Time 300 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 88.5 %TLT; ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® ST580 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® ST730 Polyester Film
DuPont Teijin Films Melinex® ST506 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® ST505 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® ST504 Polyester Film, 500 Gauge

PDTZ9254 / 139576

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.