MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Prime Polymer ULTZEX® 4050 LLDPE, Film
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Advantages: Heat Resistance; Stiffness

Major Applications: General Packaging

Information provided by Prime Polymer Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.937 g/cc0.0339 lb/in³JIS K7112
Environmental Stress Crack Resistance >= 100 hour>= 100 hourASTM D1693
Melt Flow 6.0 g/10 min6.0 g/10 minJIS K7210
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858JIS K7215
Tensile Strength at Break 25.0 MPa3630 psiJIS K7161
Tensile Strength, Yield 15.0 MPa2180 psiJIS K7161
Elongation at Break >= 500 %>= 500 %Nominal; JIS K7161
Modulus of Elasticity 0.520 GPa75.4 ksiJIS K7171
Charpy Impact, Notched NBNBJIS K7111
 
Thermal PropertiesMetricEnglishComments
Melting Point 125 °C257 °FJIS K7121
Vicat Softening Point 115 °C239 °FJIS K7206

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRIME028 / 313421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.