MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics BTU-Block ™ Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: BTU-BLOCK Ladle Liner is comprised of a waterproof version of the microporous material enclosed in a high temperature textile and quilted to form a flexible sheet.

Applications:

  • Back-up insulation in high temperature production processes – Molten metal ladles – Holding furnaces – Transfer ladles– Launders – Tundishes – Pipe wraps
  • Commercial ovens

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 0.380 MPa55.1 psiat 16 pcf, 10% deformation; ASTM C 165
 0.710 MPa103 psiat 16 pcf, 20% deformation; ASTM C 165
 1.07 MPa155 psiat 16 pcf, 30% deformation; ASTM C 165
 1.41 MPa205 psiat 16 pcf, 40% deformation; ASTM C 165
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0300 W/m-K
@Temperature 260 °C
0.208 BTU-in/hr-ft²-°F
@Temperature 500 °F
ASTM C 201
 0.0400 W/m-K
@Temperature 538 °C
0.278 BTU-in/hr-ft²-°F
@Temperature 1000 °F
ASTM C 201
 0.0500 W/m-K
@Temperature 871 °C
0.347 BTU-in/hr-ft²-°F
@Temperature 1600 °F
ASTM C 201
 0.0600 W/m-K
@Temperature 982 °C
0.416 BTU-in/hr-ft²-°F
@Temperature 1800 °F
ASTM C 201
Maximum Service Temperature, Air <= 982 °C<= 1800 °FContinuous Use
Shrinkage  0.30 %
@Treatment Temp. 538 °C,
Time 86400 sec
0.30 %
@Treatment Temp. 1000 °F,
Time 24.0 hour
ASTM C356
 0.60 %
@Treatment Temp. 815 °C,
Time 86400 sec
0.60 %
@Treatment Temp. 1500 °F,
Time 24.0 hour
ASTM C356
 1.3 %
@Treatment Temp. 954 °C,
Time 86400 sec
1.3 %
@Treatment Temp. 1750 °F,
Time 24.0 hour
ASTM C356

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6104 / 202888

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.