MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gouda Refractories Pinnacle PP 6180C3 PP Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Product Description: 80 melt flow, clarified random copolymer for injection molding. Pinnacle Polymers Polypropylene 6180C3 is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst systems to ensure uniform physical properties and lot-to-lot consistency. This product is intended for injection molding applications that require very high melt flow, more stiffness, faster cycle time, low bloom, enhanced processability and excellent clarity. This product contains a new generation clarifier.
Features: Improved FDA food contact statue; Low bloom; High melt flow, excellent processability; Reduced cycle-time; Improved color; Increased stiffness.
Pinnacle’s 6180C3 as marketed by Pinnacle Polymers Company, in natural, uncolored pellet form is cleared by way of FCN 1538 for use in single-and repeated-use articles intended to contact all types of food under the FDA Conditions of Use A-H. FDA has not evaluated the use of this product in contact with infant formula or breast milk.

Availability: Europe; North America

Additive: Clarifier

Features: Fast Molding Cycle; Food Contact Acceptable; Good Processability; High Clarity; High Flow; Low Blooming; Random Copolymer

Agency Ratings: FDA FCN 1538; FDA Food Contact

Appearance: Natural Color

Form: Pellets

Processing Method: Injection Molding

Information provided by Pinnacle Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Linear Mold Shrinkage, Flow 0.015 cm/cmASTM D955
Melt Flow 80 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4100 psi
@Thickness 3.20 mm
Injection Molded, Type I, 2.0 in/min; ASTM D638
Elongation at Break 14 %
@Temperature -17.7 °C
Injection Molded, Type I, 2.0 in/min; ASTM D638
Flexural Modulus 160000 psi
@Thickness 3.20 mm
1% Secant, Injection Molded, Type I, 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.900 ft-lb/in
@Thickness 3.20 mm
Injection Molded, Type I; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 172 °FUnannealed; ASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 9.0 %
@Thickness 1.27 mm
Yellow Index <= -10.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPINNA806 / 311499

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.