MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chesterton ARC 797 Low-viscosity, 100% solids, epoxy-based, concrete primer sealer
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Its unique hydrophobic properties allow ARC 797 to be applied to damp concrete with excellent penetrating properties. When applied, ARC 797 will improve adhesion of subsequent topcoats and reduce blistering due to out gassing associated with concrete porosity. ARC 797 is clear-to-amber in color and is non-shrinking. It is normally applied at a thickness of 0,175 mm (7 mils) to 0,250 mm (10 mils).

Application:

  • As a primer for floor coatings
  • As a sealer coat for porous concrete
  • As an adhesive for crack sealing systems

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³Cured
Viscosity 300 cP300 cP
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength >= 2.76 MPa>= 400 psiconcrete; ASTM D4541
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 50.0 °C122 °FWet Service
 65.0 °C149 °FDry Service

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asphalt
Autoclaved aerated concrete, 0.600 g/cc density
Autoclaved aerated concrete, 2.100 g/cc density
Concrete, 1-4 Dry
Concrete, clinker aggregate

PPTCHS019 / 138131

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.