MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TIMCAL TIMREX® SFG44 Primary Synthetic Graphite
Categories: Carbon; Graphite; Other Engineering Material; Additive/Filler for Polymer

Material Notes: TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.

TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.

Tribological and mechanical properties:

  • Low toughness
  • Good lubrication properties
Advantages and applications:
  • Very low friction coefficient
  • Low wear of the counterpart
  • Extreme good formation of transfer-film
  • Very high electrical conductivity
  • Excellent wettability with organic binders
  • Excellent compressibility
  • High transverse rupture strength
  • suitable for pitch-bonded, resin-bonded and metallic brushes
Information provided by TIMCAL

Key Words: CAS Number 7782-42-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.190 g/ccScott
Particle Size 5.0 µmat a density of 1.90 g/cc, pressure 2.5 t/cc
 5.0 µmSpringback 8%, pressure 0.477 t/cc
 10 µmat a density of 1.92 g/cc, pressure 2.5 t/cc
 42 µmat a density of 2.03 g/cc, pressure 2.5 t/cc
 44 - 53 µmd90, Guaranteed
 48.8 µmd90, Typical
 75 µmat a density of 2.03 g/cc, pressure 2.5 t/cc
 75 µmSpringback 6.5%, pressure 0.477 t/cc
Specific Surface Area 5.0 m²/gBET
Ash <= 0.10 %Guaranteed
 0.70 %Typical
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.750 ohm-cmparticle size 75 um, pressure 2.5 t/cc
 0.800 ohm-cmparticle size 40 um, pressure 2.5 t/cc
 1.45 ohm-cmparticle size 15 um, pressure 2.5 t/cc
 1.75 ohm-cmparticle size 10 um, pressure 2.5 t/cc
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 0.10 %Typical
 <= 0.50 %Guaranteed
 
Descriptive Properties
Crystallinity, Lc>200 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMCAL TIMREX® KS44 Primary Synthetic Graphite
TIMCAL TIMREX® KS15 Primary Synthetic Graphite
TIMCAL TIMREX® SFG15 Primary Synthetic Graphite
TIMCAL TIMREX® KS150 Primary Synthetic Graphite
TIMCAL TIMREX® KS6 Primary Synthetic Graphite

CTIMCAL38 / 2680

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.