MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC Lexan® FXD171R PC  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Transparent/transluscent PC for light diffusion special effects. MFR of 25.0.

This data was supplied by SABIC-IP for the Americas region.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D 792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC Method
Melt Flow 25 g/10 min
@Load 1.20 kg,
Temperature 300 °C
25 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 64.0 MPa9280 psiType I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 62.0 MPa8990 psiType I, 50 mm/min; ASTM D 638
Elongation at Break 125 %125 %Type I, 50 mm/min; ASTM D 638
Elongation at Yield 6.2 %6.2 %Type I, 50 mm/min; ASTM D 638
Tensile Modulus 2.33 GPa338 ksi50 mm/min; ASTM D 638
Flexural Yield Strength 93.0 MPa13500 psi1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.34 GPa339 ksi1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 7.79 J/cm
@Temperature 23.0 °C
14.6 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
Instrumented Impact Total Energy 70.0 J
@Temperature 23.0 °C
51.6 ft-lb
@Temperature 73.4 °F
ASTM D 3763
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 250 - 400 V250 - 400 VPLC code 2; UL 746A
Hot Wire Ignition, HWI 30 - 60 sec30 - 60 secPLC code 2; UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs60 - 120 arcssurface, PLC code 1; UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min1.00 - 3.15 in/minPLC code 2; UL 746A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
@Thickness 3.20 mm
279 °F
@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
@Thickness 3.20 mm
259 °F
@Thickness 0.126 in
unannealed; ASTM D 648
UL RTI, Electrical 130 °C266 °FUL 746B
UL RTI, Mechanical with Impact 130 °C266 °FUL 746B
UL RTI, Mechanical without Impact 130 °C266 °FUL 746B
Flammability, UL94 V-2
@Thickness 1.09 mm
V-2
@Thickness 0.0429 in
UL 94
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 80 %80 %transparent/translucent; thickness not quantified

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABIC2532 / 116420

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.