MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials Pearlbond® 580 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlbond™ 580 is a linear, Polyester-based TPU, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.

Application: Pearlbond™ 580 can be added to formulations of REACTIVE POLYURETHANE HOT-MELTS (HMPUR), in order to improve the crystallisation speed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 2781
Viscosity 2.70e+6 cP
@Temperature 130 °C
2.70e+6 cP
@Temperature 266 °F
Melt; ISO 1133
Melt Flow 10 - 30 g/10 min
@Load 2.16 kg,
Temperature 170 °C
10 - 30 g/10 min
@Load 4.76 lb,
Temperature 338 °F
ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 65.0 - 71.0 °C149 - 160 °FMQSA 70 A
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.15 %<= 0.15 %MQSA 44
 
Descriptive Properties
Crystallization Rate14-18 minutesMQSA 12 B
OH Value< 3 mg/KOH/gMQSA 47 A
ThermoplasticityVery HighMQSA 68A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ecomass® 4703BI62 Filled Polyurethane, Injection Molding
Huntsman IROGRAN® A 98 H 4661 Polyester-Based TPU-Injection Molding Grade
Huntsman IROGRAN® PS455-203 TPU-Polyester
Lubrizol Advanced Materials Pearlbond® 1160 Thermoplastic Polyurethane
Lubrizol ESTANE® 58224 Ester Based Thermoplastic Polyurethane

PMEQU953a / 140308

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.