MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt POLYCOR® 25-Series Polyester Resins
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: 25-Series gelcoats are formulated from premium polyester resins and fire retardant additives to achieve optimal fire retardancy properties and low slow smoke development. They are suitable for applications requiring a surface with resistance to flame spread and smoke development.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 - 1.35 g/cc0.0452 - 0.0488 lb/in³
Water Absorption 0.17 %0.17 %
Viscosity 4500 - 5000 cP4500 - 5000 cP
 10000 - 12000 cP10000 - 12000 cPbrush
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 3838
Elongation at Break 3.1 %3.1 %
 
Processing PropertiesMetricEnglishComments
Gel Time 12.0 - 15.0 min
@Temperature 22.0 °C
12.0 - 15.0 min
@Temperature 71.6 °F
100 gm mass @22°C; 1% MEC-EX

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9263 / 231858

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.