MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beryllium Copper, UNS C17200, TD04 Temper Strip
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability. Commonly fabricated by blanking, forming and bending, turning, drilling, tapping.

Applications: springs, flexible metal hose, Bourdon tubing, bellows, clips, washers, retaining rings, and other parts subject to severe forming conditions but require high strength, anelasticity, and fatigue and creep resistance; in parts that require high strength or wear resistance along with good electrical conductivity and/or magnetic characteristics such as navigational instruments, non-sparking safety tools, firing pins, bushings, valves, pumps, shafts, and rolling mill parts.

Key Words: BeCu; CDA 172, CB101, ISO CuBe2, CEN CW101C, A4/2, beryllium bronze; Alloy 25
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.25 g/ccduring age hardening, 2% max. decrease in length and 6% max. increase in density.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 96 - 102
Hardness, Rockwell C 36 - 40For rod, bar, plate and tubing, all sizes
Hardness, Rockwell 30T 79 - 83
Hardness, Vickers 200 - 260
Tensile Strength, Ultimate 1140 - 1310 MPaFor rod, bar, plate and tubing, all sizes
Tensile Strength, Yield 620 - 770 MPa
@Strain 0.2 %
Elongation at Break 2.0 - 8.0 %in 50 mm
 3.0 - 10 %For rod, bar, plate and tubing, all sizes, in 50 mm
Modulus of Elasticity 125 - 130 GPa
Poissons Ratio 0.30
Fatigue Strength 240 - 270 MPa
@# of Cycles 1.00e+8
Reverse Bending
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 40 %
Shear Modulus 50.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000010 - 0.000011 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.7 µm/m-°C
@Temperature 20.0 - 100 °C
 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
 17.8 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 105 - 130 W/m-K
@Temperature 20.0 °C
 130 - 133 W/m-K
@Temperature 200 °C
Melting Point 865 - 980 °C
Solidus 865 °C
Liquidus 980 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 845 °CHot-Shortness Temperature
Annealing Temperature 760 - 790 °C
Solution Temperature 760 - 790 °C
Aging Temperature 260 - 425 °C
Hot-Working Temperature 650 - 800 °C
Precipitation Temperature >= 600 °F
@Time 180 sec
Air
Recrystallization Temperature 730 °C
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 1.8 - 2.0 %
Co + Ni >= 0.20 %
Co + Ni + Fe <= 0.60 %
Copper, Cu 97 %
Lead, Pb <= 0.10 %
Other, total <= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Beryllium Copper, UNS C17200, TB00 Temper Strip
Beryllium Copper, UNS C17200, TF00 Temper Strip
Beryllium Copper, UNS C17200, TH04 Temper Strip
Beryllium Copper, UNS C17200, TD01 Temper Strip
Beryllium Copper, UNS C17200, TD02 Temper Strip

MC17200b5 / 10820

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.