MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® 73G50HSLA BK416 PA6-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: 50% Glass Reinforced, Heat Stabilized, Polyamide 6

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccDAM; ISO 1183
Melt Density 1.24 g/cc
@Temperature 270 °C
Water Absorption 4.5 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.60 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 150 MPa50% RH; ISO 527-1/-2
 230 MPaDAM; ISO 527-1/-2
Elongation at Break 2.2 %DAM; ISO 527-1/-2
 4.0 %50% RH; ISO 527-1/-2
Tensile Modulus 12000 MPa50% RH; ISO 527-1/-2
 16000 MPaDAM; ISO 527-1/-2
Flexural Strength 240 MPa50% RH; ISO 178
 400 MPaDAM; ISO 178
 225 MPa
@Strain 3.5 %
50% RH; ISO 178
Flexural Modulus 10000 MPa50% RH; ISO 178
 15000 MPaDAM; ISO 178
Poissons Ratio 0.3350% RH
 0.33DAM
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 100 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 18.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 19.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 21.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 22.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Tensile Creep Modulus, 1 hour 9500 MPa1h; 50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 7500 MPa1000h; 50% RH; ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 5.00e+12 ohm50% RH; IEC 62631-3-2
Comparative Tracking Index 380 VDAM; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°CDAM; ISO 11359-1/-2
Specific Heat Capacity 2.05 J/g-°C
@Temperature 270 °C
Melt
Thermal Conductivity 0.260 W/m-K
@Temperature 270 °C
Melt
Melting Point 219 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 219 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 212 °CDAM; ISO 75-1/-2
Vicat Softening Point 215 °C50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 15.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 60.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread 31.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 °COptimum, Injection
 260 - 280 °CRange, Injection
Mold Temperature 70.0 - 120 °CInjection
 100 °COptimum, Injection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA6,GF50,M1CGHR,S09-160
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA6-GF50<ISO 11469
PolymerPA6-GF50
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA6-GF50ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Thermylon® NSG-240A 50% Ceramic and Glass Fiber Reinforced Nylon 6
EMS-Grivory Grilon® BG-50 PA6-GF50
Celanese Zytel® 70G50HSLA BK039B PA66-GF50
Celanese Zytel® 73G35HSL BK262 PA6-GF35
Celanese Zytel® 73G15HSL BK363 PA6-GF15

PDSX5363 / 198003

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.