Sparkle Silver® 3333-AR is an acid resistant pigment developed for formulators requiring good face whiteness, with a fine appearance. Close packing and good distinctiveness of image (D.O.I.) make Sparkle Silver® 3333-AR a good choice for basecoat/clear automotive systems. Applications: Automotive |