MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akro-Plastic Akromid® S3 GF 15 1 black (3316) PA 6.10 Dry, 15% Glass Filled, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: Description: AKROMID S3 GF 15 1 black (3316) is a 15% glass fiber reinforced, heat stabilized polyamide 6.10 with lower moisture absorption and high chemical resistance. Applications are precision parts for apparatus engineering and precision mechanics as well as connectors, housings etc. in the automotive industry.

Additive: Heat Stabilizer

Features:

  • Good Chemical Resistance
  • Heat Stability
  • Low Moisture Absorption
  • Good Stiffness
  • Medium Strength
Uses:
  • Automotive Applications
  • Connectors
  • Engineering Parts
  • Housings

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 1183
Filler Content 15 %ISO 1172
Moisture Absorption 1.5 %
@Temperature 70.0 °C
Humidity, 62% RH; ISO 1110
Linear Mold Shrinkage, Flow 0.0060 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cmISO 294-4
Spiral Flow 45.0 cmCross section: 7 mm x 3.5 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPa5 [mm/min]; ISO 527-2
Elongation at Break 5.5 %5 [mm/min]; ISO 527-2
Tensile Modulus 5000 MPa1 [mm/min]; ISO 527-2
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 75.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 5.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CDIN EN 11357-1
Deflection Temperature at 0.46 MPa (66 psi) 220 °CUnannealed; ISO 75/B
Deflection Temperature at 1.8 MPa (264 psi) 190 °CUnannealed; ISO 75/A
Deflection Temperature at 8.0 MPa 75.0 °CUnannealed; ISO 75/C
Flammability, UL94 HB
@Thickness 0.800 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
LNP Thermocomp® DF-1004 EP BK8-250 Polycarbonate, Glass Fiber Reinforcement
Akro-Plastic Akromid® S3 GF 15 1 black (3316) PA 6.10 Conditioned, 15% Glass Filled, Heat Stabilized
LNP Thermocomp® QF-1006 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
RTP Company RTP 202B TFE 15  Nylon 6/10 (PA 6/10) Glass Fiber 15% - PTFE 15%

PAKRO356 / 182943

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.