MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion Copper Beryllium Alloy 3 Plate AT (TF00) 1.75 to 5 in (UNS C17510)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Alloys 3 plate from Materion provide high electrical and thermal conductivity coupled with moderate strength. Typical applications include resistance welding components and inserts for metal die casting, injection molding and blow molding.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 689 - 896 MPa100000 - 130000 psi
Tensile Strength, Yield 552 - 689 MPa
@Strain 0.200 %
80000 - 100000 psi
@Strain 0.200 %
Elongation at Break 8.00 - 20.0 %8.00 - 20.0 %
Modulus of Elasticity 138 GPa20000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000290 - 0.00000380 ohm-cm0.00000290 - 0.00000380 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C9.80 µin/in-°F
Thermal Conductivity 240 W/m-K1670 BTU-in/hr-ft²-°F
Melting Point 1040 °C1900 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.200 - 0.600 %0.200 - 0.600 %
Copper, Cu 97.2 - 98.4 %97.2 - 98.4 %
Nickel, Ni 1.40 - 2.20 %1.40 - 2.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBB656e / 323484

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.