MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Silberline Sil-O-Wet® 2052NL-PA
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Sil-O-Wet® grades are leafing and non-leafing aluminum pigment pastes carried in isopropyl alcohol in which the aluminum flakes have been chemically treated to reduce the aluminum-water reaction. These grades are recommended for use in aqueous flexographic and gravure ink formulations. The specific degree of gassing stability is formulation dependent and each formulation must be evaluated for acceptable stability. High or excessive shear during processing will reduce the effectiveness of the inhibitor and should be avoided.

Applications: Printing Inks; Waterborne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/cc
Volatiles 35 %
Particle Size 17 µm
 
Descriptive Properties
Aluminum Flake, wt%59
CategoryNon-leafing
SolventsIsopropyl Alcohol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

ESIBER258 / 6013

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.