MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nitriflex Nitrimpact 1300 MBS Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: NITRIMPACT™ 1300 thermoplastic resin is a methyl methacrylate-butadiene-styrene (MBS) impact modifier for transparent and opaque PVC applications.

Applications: Transparent PVC Compounds (no use restriction for translucents and opaques compounds). Used for blow moulding, extrusion, calandering, thermoforming and injection processes, for the production of artifacts like: transparent profiles, laminates in general, blister packs, tubes, hoses, automotive parts, etc.

Information provided by Dax Resinas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 0.00 - 1.0 %Method P-020
 
Mechanical PropertiesOriginal ValueComments
Izod Impact, Notched 1200 J/m
@Thickness 6.35 mm
ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Denka TP-803 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
INEOS Styrolution Zylar® 650 MBS
Denka TP-802 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
INEOS Styrolution Zylar® 960 MBS
Denka TH-11 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene

PDAX076 / 29501

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.