Product Description: A nucleated impact copolymer resin with medium flow, high stiffness and antistatic properties. It is suitable for molding applications like consumer products, closures, containers, toys and rigid packaging applications. Availability: Africa & Middle East and Europe Features: - Antistatic
- Good Flow
- High Stiffness
- High Crystalline
- Nucleated
Uses: - Construction Applications
- Crates
- Industrial Applications
- Pails
- Tool/Tote Box
- Toys
Processing Method: Injection Molding and CompoundingInformation provided by ExxonMobil |