MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Resin Technology Group TIGA 905 One-Part Silver Conductive Epoxy System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Electrically Conductive

Material Notes: Cure 6 minutes at 130°C or 3 minutes at 150°C.

TIGA 905 is a stress-absorbing and electrically conductive, silver-filled epoxy adhesive recommended for solder replacement in microelectronic interconnect applications. This one-part, smooth paste formulation of refined pure silver and epoxy develops strong, durable, electrically and thermally conducting bonds and coatings between many different and dissimilar materials such as metals, ceramics, glass and plastic laminates. TIGA 905 is screen printable, and capable of in line surface mount component attach assembly operations.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.60 g/cc3.60 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Shear Strength 10.3 MPa1500 psiCured 6 minutes at 130°C, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.00040 ohm-cm0.00040 ohm-cmCured 6 minutes at 130°C
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  3.00 min
@Temperature 150 °C
0.0500 hour
@Temperature 302 °F
 6.00 min
@Temperature 130 °C
0.100 hour
@Temperature 266 °F
Pot Life 1440 min1440 min
 
Descriptive Properties
ColorSilver
ViscositySmooth pasteAfter mixing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESINT601 / 65485

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.