MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LATI LATISTAT 49/2000-01 Elastomer Modified Polypropylene (Epm) Base Conductive Plastic  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polypropylene (PP)

Material Notes: Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable mechanical properties. The LATISTAT compounds are used in all applications where product surface must be completely and permanently free of static charges. Addition of carbons supplying electric semi-conductivity will diminish the flowability and good surface finish of the materials, and limiting the prospects of obtaining colored products.

Applications: cabinets, containers, boxes for storage and handling of discharge-sensitive electronic components, casings and bodies for electrical and mechanical components to be used in areas where flammable and explosive materials are processed, parts for typewriters, printers, photocopiers, parts for textile machinery, racks and tracks for printed circuits; electro-medical equipment.

Specific Notes for this Material: elastomer modified polypropylene base (EPm); very low specific resistivity; good flexibility and impact resistance.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Linear Mold Shrinkage 0.010 cm/cmLATI
Linear Mold Shrinkage, Transverse 0.010 cm/cmLATI
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 0.900 GPaASTM D790
Izod Impact, Notched 400 J/m
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistance <= 100 ohmIEC 93
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 230 °C
Mold Temperature 30.0 - 50.0 °C
Drying Temperature 80.0 - 90.0 °CTemperature can be reduced when using vacuum ovens.
Dry Time >= 3 hourDrying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Injection Speedmedium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic
Lehmann & Voss LUVOCOM® 1301-0915 PPS, linear with carbon fiber, PTFE, lubricant modified
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide with carbon fiber and PTFE
LATI LATISHIELD 87/30-06A-V0 Polycarbonate E.M.I. Shielding Plastic

PLATI217 / 50215

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.