MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beryllium Copper, UNS C17000, TM02 Temper Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability. Commonly fabricated by blanking, forming and bending, turning, drilling, tapping.

Applications: bellows, bourdon tubing, diaphragms, fuse clips, fasteners, lock-washers, springs, switch parts, roll pins, valves, welding equipment.

Available as flat products, rod.

Proprietary mill heat treatment intended to produce the stated tensile properties.

Key Words: BeCu; 165 Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.26 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C >= 25
Hardness, Rockwell HR30N 46 - 50
Hardness, Vickers 260 - 295
Tensile Strength, Ultimate 825 - 930 MPa
Tensile Strength, Yield 690 - 860 MPa
@Strain 0.2 %
Elongation at Break 12 - 16 %in 50 mm
Modulus of Elasticity 115 GPa
Poissons Ratio 0.30
Fatigue Strength 240 - 270 MPa
@# of Cycles 1.00e+8
rotating beam
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 50.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000052 - 0.0000086 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.7 µm/m-°C
@Temperature 20.0 - 100 °C
 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
 17.8 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 118 W/m-K
 145 W/m-K
@Temperature 200 °C
Melting Point 865 - 980 °C
Solidus 865 °C
Liquidus 980 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 845 °CHot-Shortness Temperature
Annealing Temperature 775 - 800 °C
Solution Temperature 760 - 790 °C
Aging Temperature 260 - 425 °C
Hot-Working Temperature 650 - 825 °C
Recrystallization Temperature 730 °C
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 1.6 - 1.79 %
Co + Ni >= 0.20 %
Co + Ni + Fe <= 0.60 %
Copper, Cu 98.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Beryllium Copper, UNS C17000, TM00 Temper Strip
Beryllium Copper, UNS C17000, TM01 Temper Strip
Beryllium Copper, UNS C17000, TM04 Temper Strip
Beryllium Copper, UNS C17000, TH01 Temper Strip
Phosphor bronze 5% Sn, UNS C51000, H08 Temper flat products

MC17000c3 / 10731

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.